Aging Management Guidance to Address Potential Chloride-Induced Stress Corrosion Cracking of Welded Stainless Steel Canisters

Description
EPRI report to assess the susceptibility of the welded stainless steel canisters used in dry cask storage systems to aging-related degradation mechanisms, specifically chloride-induced stress corrosion cracking.
Content Originator
Information Type
Location
Key Element
Date
9 years 5 months ago